Hot In-Place Recycling
Find a Contractor/Supplier

Pre-Construction Testing

Evaluation of Existing Pavement Structure If pavement distresses suggest weak subgrade or if traffic levels are forecast to increase, check the strength of pavement and subgrade layers with falling weight deflectometer (FWD) or Dynamic Cone Penetrometer (DCP) Recommended
Ground Penetrating Radar (GPR) Verify thickness of existing asphalt and granular layers Optional
Pavement Sampling Obtain pavement cores for mix design and verify thickness of asphalt layers and presence and depth of geosynthetics Required
Mix Design Perform mix design in accordance with agency requirements Required
Measure existing slope/cross fall Ensure HIR can be constructed per contract requirements  

Cores should be checked for the presence of paving fabrics and should be at least 1 inch below the anticipated HIR depth.


Construction Testing

 

 

 

Surface Recycling

Remixing

Repaving

Rejuvenating Agent

Supplier generated COA or laboratory testing to comply with mix design parameters

Recommended

Recommended

Recommended

Rejuvenating Agent Temperature

Probe or infrared temperature gun

Recommended

Recommended

Recommended

Rejuvenating Agent Injection Rate

 

Verify amount of rejuvenating agent per mix design and accuracy of meter readings by

volumetric distribution

Required

Required

Required

Corrective HMA/

Aggregate Gradation

Supplier generated COA or laboratory analysis

(AASHTO T 11 and  T 27 or

ASTM C117 and C136)

N/A

Required

N/A

Corrective Aggregate Physical Properties

Supplier generated COA or laboratory analysis

(AASHTO T 96, T 176 and T 85 or  ASTM C131, D2419 and  C127)

N/A

Recommended

N/A

Corrective HMA Mixture Properties

Supplier generated COA or laboratory analysis

(Agency HMA Requirements)

N/A

Required

N/A

Corrective Aggregate/ HMA Addition Rate

Volumetric distribution

N/A

Required

N/A

New HMA Mix Properties

Agency HMA Requirements

N/A

N/A

Required

Ambient Temperature

Any Owner Agency approved method

Required

Required

Required

Depth of HIR Treatment

Depth probe measurement

Required

Required

Required

Recycled Mixture Temperature

Probe or infrared temperature gun (behind screed)

Require

Required

Required

Control Strip

Nuclear gauge per

AASHTO T 355 (ASTM D2950) or Owner Agency approved method

Recommended

Recommended

Recommended

Recycled Material Compacted Density

Nuclear gauge AASHTO T 355 (ASTM D2950) or Owner Agency approved method

Required

Required

Required

 


Post-Construction Testing

Cross-slope 6 ft. (1.8 m) Smart level Required
Mat Width Tape measurement Required
Surface Tolerance 10 ft. (3 m) Straight edge Recommended